Search This Supplers Products:Thermal Laminating FilmHot Stamping FoilLaminating MachineUV VarnishMetalized Laminating FilmHologram Film
US $3819.002 - 6 metric ton
US $3756.007 - 13 metric ton
Paramtents
Corona Treatment One or double sides
Thickness 24micron
Width 180mm to 1200mm
Length 2000m,3000m,4000m
Paper Core 1 or 3 inch
Packaging By carton or pallet
Delivery Lead 25 days
Type Glossy or Matte
Packging & Delivery
Min Order2 metric ton
Briefing
Detailed
* Metalized Lamination Film is applied to Books,Posters,Presentation Folders,Labels,Shopping Bag,POP Signs,Document,Book Covers,ID Cards,License,Passports,Antigraffiti,Boardmaking,Write on/wipe off Calendars,Photographs,Albums ect.
* Outside coating for wrapping box or bag for food,medicine,cosmetic,gift,liquor etc.
* Drawing paper,documents,advertisement,digital printing,show board,etc.
Guide on operation
1. Better to be used by dry/heat laminator.
2. Adjust roller pressure and temperature according to different types of paper and ink.
3. When using the film for the first time or changing the usual size, a small trial volume before starting massive lamination is proposed.
4. Normal process temperature is 90C-105C (203F - 221F), roller pressure and temperature vary from different types of paper, ink and machines.
5. Make sure the ink is dry before laminating. It will delaminate when the paper contains too much moisture or powder.
6. Make sure to put the material in place with low temperature and dry.
7. The following situation will affect the final quality of the film during lamination.
A. Using metal ink
B. Ink containing too much wax, dried oil, adhesive, silicon additive and so on.
C. Much too thick ink
D. Ink completely undried yet.
E. Much too humid paper sheet
F. Too much powder on the surface