Follow us :

High-gloss Silk-Screen UV Varnish

High-gloss Silk-Screen UV Varnish
group name
UV Varnish
Min Order
1 ton
brand name
Huanyuan
model
AFP-UV9301
Nearest port for product export
Xiamen, Ningbo, Shanghai
Delivery clauses under the trade mode
FOB, CFR, CIF, EXW, DDP, DDU, Express Delivery
Acceptable payment methods
T/T, L/C, MoneyGram, Credit Card, PayPal, Westem Union, Cash, Escrow
Export mode
Have the independent export and import right
update time
Fri, 04 Jan 2013 21:07:27 GMT

Paramtents

  • Viscosity 32000-4000mpa.s(25°C,3#30r/min)

  • Appearance Milky half-transparent or turbid thick liquid

  • Solid Content ≥95.0(UV cured, 120C*1h)

  • Standard Toy security and health

  • Package By iron cans

  • Net Weight 5kgs

  • Shelf Life 6 months

  • Curing Speed 10-15m/min (80w/cm, 1light)

Packging & Delivery

  • Min Order1 ton

Briefing

*Curable UV varnish with high gloss
*Good abrasion resistance
*Applicable for spot UV varnish for corona treated BOPP film

Detailed

AFP-UV9301High-gloss Silk-Screen UV Varnish 

***Product profile
AFP-UV9301 is an UV curable varnish with high glossmade up with imported raw materials
including acry
latesmonomers with functional groups and additives. It has ex
cellent
pe
rformance including high gloss, good adhesion, high slippy and good abrasion resistance
.
No solvent inside and meets the Toy Security and Health Standard.
AFP-UV9301 is applicable as spot UV varnish for corona treated BOPP with surface tension higher than 40. 

*** Specifications
1.Appearance: milky half-transparent or turbid thick liquid
2.Viscosity: 2000-4000mpa.s(25°C, 3#30r/min)
3.Solid content:95.0(UV cured, 120C*1h)
4. Curing speed: 1 0-15m/min (80w/cm, light)  

***Usage recommendation
1. It can be applied by 250-420 mesh silk-screen directly, not easy to block
2. If the liquid is toothick to flow, diluted by 5-10 particular thinner 

***Notice
1.Stirring before use, make sure ingredients inside mixed equally
2.Store in cool, dry, shady and air-circulative places, keep it sealed. Apply it by 250-420
mesh screen
3. Avoid contacting with skindirectly. Wash skin immediately by soap if contacted with the
varnish.
4. Since conditions can be different, uring speed and adhesion after cured should be tested
in advance
. Pay attention if ink dried completely
5. Clean by cleaner liquid immediately after printing finished. Only restart after all solvent
goes away
6. Special attention must be paid that this BOPP varnish and not be mixed with other UV
varnish or ink together
7. All the data above are acquired in the lab. Because of different substrates, ink and process, the data can be different. Customer needs to test before put in use and decide the applicability by himself 